Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 180.00 MPa @Strain 0.200 % |
26107 psi @Strain 0.200 % |
as cast |
Wieland Portagold Casting Alloy Gold casting alloyApplications: inlays/onlays, crownsDental |
|||
Tensile Strength, Yield | 180.00 MPa @Strain 0.200 % |
26107 psi @Strain 0.200 % |
hardened |
Wieland Portagold Casting Alloy Gold casting alloyApplications: inlays/onlays, crownsDental |