Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 123 MPa @Strain 0.200 %, Temperature 400 °C |
17800 psi @Strain 0.200 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |