Polymer Property : Tensile Strength, Yield = 176 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 176 MPa

@Strain 0.200 %,
Temperature 100 °C
25500 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel
Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C..
Tensile Strength, Yield 176 MPa

@Strain 0.200 %,
Temperature 100 °C
25500 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4550 Austenitic Stainless Steel
Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto) and rod forms.
Tensile Strength, Yield 176 MPa

@Thickness 1.57 mm
25500 psi

@Thickness 0.0620 in
LW; ASTM D638
Industrial Laminates/Norplex NP613 Paper Base Laminate
Description: NP613 is constructed from electrical grade of kraft paper and a specially modified epoxy resin system. It is designed to be used in tap changers, coil support plates and terminal panels..