Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 165.1 MPa @Strain 10.0 % |
23950 psi @Strain 10.0 % |
ASTM D95 |
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Machined Parts Superior chemical property, very high radiation resistance, electrical and thermal property, low outgassing and superior physical propertyInformation provided by Daelim H&L |