Polymer Property : Tensile Strength, Yield = 16400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 113 MPa

@Strain 0.200 %,
Temperature 500 °C
16400 psi

@Strain 0.200 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..