Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 164 MPa @Strain 1.00 %, Temperature 400 °C |
23800 psi @Strain 1.00 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 164 MPa @Strain 1.00 %, Temperature 400 °C |
23800 psi @Strain 1.00 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms. |
|||
Tensile Strength, Yield | 164 MPa @Strain 1.00 %, Temperature 400 °C |
23800 psi @Strain 1.00 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |