Polymer Property : Tensile Strength, Yield = 16.08 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.08 MPa

@Strain 300 %
2332 psi

@Strain 300 %
ASTM D1708
DSM Biomedical PurSil® AL 5 Aliphatic Thermoplastic Silicone Polyether Urethane  (discontinued **)
PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether..