Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1093 MPa @Strain 0.200 %, Thickness 3.20 mm |
158500 psi @Strain 0.200 %, Thickness 0.126 in |
40% cold reduction |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Yield | 1093 MPa @Temperature 23.0 °C |
158500 psi @Temperature 73.4 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 30% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |