Mechanical Properties Metric English Comments
Tensile Strength, Yield 156 MPa

@Strain 1.00 %,
Temperature 400 °C
22600 psi

@Strain 1.00 %,
Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 156 MPa

@Strain 1.00 %,
Temperature 300 °C
22600 psi

@Strain 1.00 %,
Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 156 MPa

@Strain 1.00 %,
Temperature 300 °C
22600 psi

@Strain 1.00 %,
Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 156 MPa

@Strain 1.00 %,
Temperature 400 °C
22600 psi

@Strain 1.00 %,
Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel
Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C..
Tensile Strength, Yield 156 MPa

@Temperature 649 °C
22600 psi

@Temperature 1200 °F
ASTM E8
ATI Allegheny Ludlum 310 Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..