Mechanical Properties Metric English Comments
Tensile Strength, Yield 106.0 MPa

@Strain 10.0 %
15380 psi

@Strain 10.0 %
ASTM D95
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Direct Formed  (Unverified Data**)
Information provided by Daelim H&L