Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 151 MPa @Strain 0.200 %, Temperature 1000 °C |
21900 psi @Strain 0.200 %, Temperature 1830 °F |
Bar |
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |