Polymer Property : Tensile Strength, Yield = 1500 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1500 MPa

@Temperature -3.89 °C
218000 psi

@Temperature 25.0 °F
International Mold Steel DH21 Die Cast & Forging Steel
DH21 is for aluminum die cast dies.Information provided by International Mold Steel
Tensile Strength, Yield 1500 MPa

@Strain 0.200 %
218000 psi

@Strain 0.200 %
80% Reduction of Section
Schmolz + Bickenbach LeanDupâ„¢ 35N Stainless Steel Bar
Description: LeanDupâ„¢ 35N also known as (Uranus 35 N) is a dual phase austentic-ferritic stainless steel that has the ability to become as important as 316L. It offers better corrosion resistan..