Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 146 MPa @Temperature 649 °C |
21200 psi @Temperature 1200 °F |
|
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated.. |
|||
Tensile Strength, Yield | 146 MPa @Temperature 760 °C |
21200 psi @Temperature 1400 °F |
|
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated.. |
|||
Tensile Strength, Yield | 146 MPa @Temperature 427 °C |
21200 psi @Temperature 801 °F |
|
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated.. |