Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1370 MPa @Strain 0.200 % |
198000 psi @Strain 0.200 % |
44-48 HRC |
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica.. |