Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.32 MPa @Strain 300 % |
1350 psi @Strain 300 % |
ASTM D412 |
SK Chemicals SKYTHANE® 180A R series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 9.32 MPa @Strain 100 % |
1350 psi @Strain 100 % |
ASTM D412 |
SK Chemicals SKYTHANE® 190A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 9.30 MPa @Strain 10.0 % |
1350 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® PM471 45 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 9.30 MPa @Strain 10.0 % |
1350 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® PM471 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 9.30 MPa @Strain 5.00 % |
1350 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® PM581 58 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 9.30 MPa @Strain 5.00 % |
1350 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® PM581 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |