Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1330 MPa @Strain 0.200 % |
193000 psi @Strain 0.200 % |
48 HRC |
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel Description: Thermodur® 2367 Superclean is an electro slag remelted (ESR) hot work die steel developed for applications where high temperature properties (tensile strength & thermal conductivity).. |