Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1312 MPa @Strain 0.200 %, Thickness 3.20 mm |
190300 psi @Strain 0.200 %, Thickness 0.126 in |
60% cold reduction |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |