Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 880 MPa @Temperature 500 °C |
128000 psi @Temperature 932 °F |
|
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel Description: DH2F is one of the best machining pre-hardened H13-type steels available.Unique Characteristics: 38-42 HRc hardness.Through hardened for exceptional dimensional stability.Cuts mold maki.. |