Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 860 MPa

@Strain 0.200 %
>= 125000 psi

@Strain 0.200 %
H1075 Condition - 580°C at 4 hr
Latrobe Lescalloy® 17-4 VAC-ARC Precipitation Hardening Stainless Steel
LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe..
Tensile Strength, Yield 860 MPa

@Strain 0.200 %,
Temperature 540 °C
125000 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for..
Tensile Strength, Yield 862 MPa

@Temperature -55.0 °C
125000 psi

@Temperature -67.0 °F
90°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber
Information provided by HexCel
Tensile Strength, Yield 862 MPa

@Strain 0.200 %
125000 psi

@Strain 0.200 %
H1150
Crucible Steel 15-5 Precipitation Hardening Stainless Steel
Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V..
Tensile Strength, Yield 862 MPa

@Strain 0.200 %
125000 psi

@Strain 0.200 %
H1150
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a..
Tensile Strength, Yield 862 MPa

@Strain 0.200 %
125000 psi

@Strain 0.200 %
H1150
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. ..
Tensile Strength, Yield 862 MPa

@Strain 0.200 %
125000 psi

@Strain 0.200 %
Tempering Temperature-1200°F
Crucible Steel 422 Stainless Steel
Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is..