Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 854 MPa @Strain 0.200 % |
124000 psi @Strain 0.200 % |
Typical, Longitudinal Direction |
Industeel CLC 1.2311 Prehardened Mold Steel (300HB/30HRC) Description: CLC 1.2311 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, carbon and manganese additions are optimized to have a fully martens.. |
|||
Tensile Strength, Yield | 855 MPa @Temperature 24.0 °C |
124000 psi @Temperature 75.2 °F |
Dry |
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |
|||
Tensile Strength, Yield | 855 MPa @Temperature 71.0 °C |
124000 psi @Temperature 160 °F |
Dry |
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |