Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 841 MPa @Temperature 23.0 °C |
122000 psi @Temperature 73.4 °F |
AS4C; Fill Tension; (AMB) |
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form Fibers: T300-3K, AS4C-3KInformation provided by HexCel |
|||
Tensile Strength, Yield | 843 MPa @Temperature 23.0 °C |
122000 psi @Temperature 73.4 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 20% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |