Tensile Strength, Yield 8.20 MPa

@Strain 50.0 %
1190 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 2095A Poly(caprolactone)ester TPU Resin
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi..