Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 7.85 MPa @Strain 10.0 % |
1140 psi @Strain 10.0 % |
ASTM D638 |
Samyang Triel® 5501BM Thermoplastics Polyetherester Elastomer, Blow Molding Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5501BM is for blow molding applications.Applications: Automotive BellowsInformation provided by Samyang... |
|||
Tensile Strength, Yield | 7.85 MPa @Strain 300 % |
1140 psi @Strain 300 % |
ASTM D412 |
SK Chemicals SKYTHANE® 420 Hotmelt Grade UB Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |