Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 1140 MPa @Strain 0.200 % |
>= 165000 psi @Strain 0.200 % |
H1050 Condition - 565°C |
Latrobe Lescalloy® 13-8 Mo VIM-VAR Precipitation Hardening Stainless Steel Lescalloy 13-8 Mo VIM-VAR is a precipitation hardening martensitic stainless steel offering excellent fracture toughness and transverse mechanical properties coupled with the resistance to stress-co.. |