Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1090 MPa @Strain 0.200 % |
158000 psi @Strain 0.200 % |
|
PSM Industries PolyAlloys MIM-14-4PH Heat Treated Stainless Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Yield | 1090 MPa @Temperature 25.0 °C |
158000 psi @Temperature 77.0 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 1090 MPa @Strain 0.200 % |
158000 psi @Strain 0.200 % |
57.8% Cold Work |
AK Steel NITRONIC® 19-D Duplex Stainless Steel AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}),
good drawing and welding characteristi.. |