Mechanical Properties Metric English Comments
Tensile Strength, Yield 731 MPa

@Strain 0.200 %
106000 psi

@Strain 0.200 %
PSM Industries PolyAlloys MIM-17-4PH sintered Stainless Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..
Tensile Strength, Yield 730 MPa

@Temperature 600.0 °C
106000 psi

@Temperature 1112 °F
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel
Description: DH2F is one of the best machining pre-hardened H13-type steels available.Unique Characteristics: 38-42 HRc hardness.Through hardened for exceptional dimensional stability.Cuts mold maki..
Tensile Strength, Yield 731 MPa

@Strain 0.200 %
106000 psi

@Strain 0.200 %
4 in. Test Specimen
Latrobe Lescalloy® 410Cb High Strength Stainless Steel
LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe..
Tensile Strength, Yield 733 MPa

@Temperature 25.0 °C,
Time 11500 sec
106000 psi

@Temperature 77.0 °F,
Time 3.20 hour
As Welded and Aged at 1850°F(1010°C)/2hr/AC + 1450°F(788°C)/8h/AC; Base/Weld Fracture; 0.2% Offset
Haynes 282® Nickel Alloy Autogenously Welded Sheet
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Tensile Strength, Yield 731 MPa

@Strain 2.00 %,
Temperature 538 °C
106000 psi

@Strain 2.00 %,
Temperature 1000 °F
H900
Crucible Steel 15-5 Precipitation Hardening Stainless Steel
Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V..
Tensile Strength, Yield 731 MPa

@Strain 2.00 %,
Temperature 538 °C
106000 psi

@Strain 2.00 %,
Temperature 1000 °F
H900
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a..
Tensile Strength, Yield 731 MPa

@Strain 2.00 %,
Temperature 538 °C
106000 psi

@Strain 2.00 %,
Temperature 1000 °F
H900
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. ..