Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 717 MPa @Temperature 427 °C |
104000 psi @Temperature 801 °F |
|
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt.. |
|||
Tensile Strength, Yield | 717 MPa @Strain 0.200 % |
104000 psi @Strain 0.200 % |
Typical for Plate, 1/4-Hard, Longitudinal, 0.1875' |
AK Steel NITRONIC® 30 Austenitic Stainless Steel AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi.. |
|||
Tensile Strength, Yield | 716 MPa @Temperature 23.0 °C |
104000 psi @Temperature 73.4 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 10% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Tensile Strength, Yield | 718 MPa @Treatment Temp. 718 °C, Time 3.60e+6 sec |
104000 psi @Treatment Temp. 1320 °F, Time 1000 hour |
0.2%. Room temp test after thermal exposure |
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |
|||
Tensile Strength, Yield | 715 MPa @Strain 0.200 %, Temperature 25.0 °C |
104000 psi @Strain 0.200 %, Temperature 77.0 °F |
|
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |