Mechanical Properties Metric English Comments
Tensile Strength, Yield 1030 MPa

@Strain 0.200 %
150000 psi

@Strain 0.200 %
40-42 HRC
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel
Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica..
Tensile Strength, Yield 1030 MPa

@Strain 0.200 %
150000 psi

@Strain 0.200 %
H1075
Crucible Steel 15-5 Precipitation Hardening Stainless Steel
Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V..
Tensile Strength, Yield 1030 MPa

@Strain 2.00 %,
Temperature 316 °C
150000 psi

@Strain 2.00 %,
Temperature 600 °F
H900
Crucible Steel 15-5 Precipitation Hardening Stainless Steel
Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V..
Tensile Strength, Yield 1030 MPa

@Strain 0.200 %
150000 psi

@Strain 0.200 %
H1075
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a..
Tensile Strength, Yield 1030 MPa

@Strain 2.00 %,
Temperature 316 °C
150000 psi

@Strain 2.00 %,
Temperature 600 °F
H900
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a..
Tensile Strength, Yield 1030 MPa

@Strain 0.200 %
150000 psi

@Strain 0.200 %
H1075
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. ..
Tensile Strength, Yield 1030 MPa

@Strain 2.00 %,
Temperature 316 °C
150000 psi

@Strain 2.00 %,
Temperature 600 °F
H900
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. ..