Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.998 MPa @Temperature 21.1 °C |
1015 psi @Temperature 70.0 °F |
Flatwise Tension |
Hexcel® Redux® 322 Modified epoxy film adhesive (0.06 psf) Redux 322 is a high performance modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures, where operating temperatures are experienced up .. |
|||
Tensile Strength, Yield | 6.998 MPa @Temperature 149 °C |
1015 psi @Temperature 300 °F |
Flatwise Tension |
Hexcel® Redux® 322U Modified epoxy film adhesive (0.06 psf) Redux 322 is a high performance modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures, where operating temperatures are experienced up .. |