Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 12.0 - 18.0 x 10-8 mm³/N-M
5.96 - 8.94 x 10-10 in³-min/ft-lb-hr
at PV 100; ASTM D3702
Guarniflon PTFE G456 Polytetrafluoroethylene 25% Hard Carbon
PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w..