Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 10.0 - 142 x 10-8 mm³/N-M | 4.96 - 70.6 x 10-10 in³-min/ft-lb-hr | Average value: 39.6 x 10<sup>-8</sup> mm³/N-M Grade Count:8 |