Mechanical Properties Metric English Comments
K (wear) Factor 135 x 10-8 mm³/N-M
67.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66
LNP* LUBRICOMP* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
K (wear) Factor 135 x 10-8 mm³/N-M
67.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66 (Asia Pacific)
LNP* Lubricomp* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.