Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 65.0 x 10-8 mm³/N-M
32.3 x 10-10 in³-min/ft-lb-hr
LATI Latilub 37 B01-02S Bio-Polymer
Self-lubricating product based on Bio-Polymer (PLA, PHB, ...). Silicone.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..