Polymer Property : K (wear) Factor = 6.80 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 6.80 - 353 x 10-8 mm³/N-M
3.38 - 175 x 10-10 in³-min/ft-lb-hr
Average value: 184 x 10<sup>-8</sup> mm³/N-M Grade Count:4
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
K (wear) Factor 6.80 x 10-8 mm³/N-M
3.38 x 10-10 in³-min/ft-lb-hr
LATI Latilub 88/10-15T G/30 PEEK, 30% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..