Polymer Property : K (wear) Factor = 5.10 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 5.10 - 50.4 x 10-8 mm³/N-M
2.53 - 25.0 x 10-10 in³-min/ft-lb-hr
Average value: 20.3 x 10<sup>-8</sup> mm³/N-M Grade Count:11
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
K (wear) Factor 5.10 x 10-8 mm³/N-M
2.53 x 10-10 in³-min/ft-lb-hr
LATI Latilub 66-20T G/40 PA66, 40% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri..