Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 4.70 x 10-8 mm³/N-M | 2.33 x 10-10 in³-min/ft-lb-hr | |
LATI Latilub 80-40GRT PPS, Graphite/PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). Graphite / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
K (wear) Factor | 4.70 x 10-8 mm³/N-M | 2.33 x 10-10 in³-min/ft-lb-hr | |