Mechanical Properties Metric English Comments
K (wear) Factor 79.2 x 10-8 mm³/N-M
39.3 x 10-10 in³-min/ft-lb-hr
at 5000 psi - fpm PV; ASTM D3702
3M Dyneon™ CC604 PTFE, 20% Fiberglass Filled  (discontinued **)
Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon.