Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 308 x 10-8 mm³/N-M | 153 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DP001E PC LNP* LUBRICOMP* DP001E is a Polycarbonate base resin containing 5% PTFE/Silicone. Added features are: Internally Lubricated, Easy Molding. |