Mechanical Properties Metric English Comments
K (wear) Factor 2900 x 10-8 mm³/N-M
1440 x 10-10 in³-min/ft-lb-hr
at PV 100; ASTM D3702
Guarniflon PTFE G400 Polytetrafluoroethylene
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif..