Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 469 x 10-8 mm³/N-M | 233 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp ML002S PP LNP* Lubricomp* ML002S is a compound based on Polypropylene containing PTFE. Characteristics of this grade are: Heat Stabilized and Internally Lubricated.This data was supplied by SABIC-IP for the.. |