Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 228 x 10-8 mm³/N-M | 113 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP ZFG26 PPE+PS LNP* LUBRICOMP* ZFG26 is a compound based on PPE+PS resin containing 30% Glass Fiber, 10% Graphite. Added features of this material include: Wear Resistant. |
|||
K (wear) Factor | 228 x 10-8 mm³/N-M | 113 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP ZFG26 PPE+PS (Asia Pacific) LNP* Lubricomp* ZFG26 is a compound based on PPE+PS Blend resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |