Mechanical Properties Metric English Comments
K (wear) Factor 209 x 10-8 mm³/N-M
104 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RI001 PA 66
LNP* LUBRICOMP* RI001 is a compound based on Nylon 66 resin containing 2% Silicone. Added feature of this grade is: Wear Resistant.