Polymer Property : K (wear) Factor = 1610 x 10
-8
mm³/N-M
Polymer Property :
K (wear) Factor =
1610 x 10
-8
mm³/N-M
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
K (wear) Factor
1610
x 10
-8
mm³/N-M
800
x 10
-10
in³-min/ft-lb-hr
QTM 55010
Quadrant EPP Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet)