K (wear) Factor 15.5 x 10-8 mm³/N-M
7.70 x 10-10 in³-min/ft-lb-hr
K=W/PVT where W=wear (inches^3); P=applied pressure (psi); V=velocity (fpm); T=time (hours).
A. Schulman ComAlloy Lubrilon® 636 Nylon 6/6, Carbon Fiber Reinforced, Proprietary Lubricant Package
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..