Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 125 x 10-8 mm³/N-M | 62.0 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Techtron® HPV PPS (ASTM Product Data Sheet) |
|||
K (wear) Factor | 125 x 10-8 mm³/N-M | 62.0 x 10-10 in³-min/ft-lb-hr | PV=2000 psi-fpm vs Self; SABIC Method |
SABIC Innovative Plastics ULTEM 4000 PEI Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |
|||
K (wear) Factor | 125 x 10-8 mm³/N-M | 62.0 x 10-10 in³-min/ft-lb-hr | PV=2000 psi-fpm vs Self; SABIC Method |
SABIC Innovative Plastics ULTEM 4000 PEI (Asia Pacific) Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |