K (wear) Factor 100 x 10-8 mm³/N-M
49.6 x 10-10 in³-min/ft-lb-hr
LATI Latilub 30/R-07GRT PC, Graphite/PTFE Reinforced
Self-lubricating product based on Polystyrene (PS). Graphite / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termo..