Mechanical Properties Metric English Comments
K (wear) Factor 22.0 x 10-8 mm³/N-M
10.9 x 10-10 in³-min/ft-lb-hr
LATI Latilub 75/4-05T G/30-V0 PBT, 30% Glass Fiber Reinforced, PTFE Filled, Flame Retardant
Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Afri..