Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 3.22 x 10-8 mm³/N-M | 1.60 x 10-10 in³-min/ft-lb-hr | Lubricated: 0.375 m/s, 6.9 MPa (75 fpm, 1000 psi); ASTM D3702 |
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications. Torlon PAI has the highest.. |