Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 0.604 x 10-8 mm³/N-M | 0.300 x 10-10 in³-min/ft-lb-hr | Lubricated: 4 m/s, 5.2 MPa (800 fpm, 750 psi); ASTM D3702 |
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications. Torlon PAI has the highest.. |