Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 59.3 MPa | 8600 psi | ASTM D790 |
ExxonMobil Vistamaxx™ 3000 Propylene-based Elastomer Product Description: Vistamaxx 3000 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Technology. It has moderate elastomeric properties, is easy to .. |